• română
    • English
    • français
    • Deutsch
    • español
    • italiano
  • română 
    • română
    • English
    • français
    • Deutsch
    • español
    • italiano
  • Logare
Vezi articolul 
  •   Pagina principală
  • Scientific papers - Annals of "Dunarea de Jos" University of Galati - Analele științifice ale Universității "Dunărea de Jos" din Galați
  • Fascicula IX
  • 1993 -2018
  • 2008 fascicula9 nr1
  • Vezi articolul
  •   Pagina principală
  • Scientific papers - Annals of "Dunarea de Jos" University of Galati - Analele științifice ale Universității "Dunărea de Jos" din Galați
  • Fascicula IX
  • 1993 -2018
  • 2008 fascicula9 nr1
  • Vezi articolul
JavaScript is disabled for your browser. Some features of this site may not work without it.

Mass Erosion and Material Transfer at the Deposition of Layers by Inverse Electroerosion

Thumbnail
View/Open
ugal_f9_2008_8Alexandru.pdf (926.1Kb)
Dată
2008
Autor
Alexandru, Adrian
Huţanu, Marius
Iacob Strugaru, Sorin
Metadata
Arată înregistrarea completă a articolului
Abstract
The deposition and alloying of the superficial layers by inverse electroerosion or by electric spark given by a vibrating electrode permits to obtain a large scale of properties at the surface of metallic materials from tools, machines organs, electric contacts, etc. During the inverse electroerosion, the evaporated and ionizated material from electrode (+) under the influence of temperature and electric field, is transferred and deposed on the surface of the part (-). The intensity of material transfer depends on the parameters of the electrical discharge between electrodes, on the time of work and on the nature of the electrodes. This paper work wants to establish the type of evolution in time of the quantity of erodated material from electrode and deposed on the surface of the part. The experimental results are in accordance with the theory of the phenomena of erosion by temperature mixed with the phenomena of massic erosion. The results show that the deposed mass increases by the specific time of deposition until it reaches maxim value, then it decreases.
URI
http://10.11.10.50/xmlui/handle/123456789/5601
Colecții
  • 2008 fascicula9 nr1 [22]

DSpace 6.0 | Copyright © Arthra Institutional Repository
Contactați-ne | Trimite feedback
Theme by 
Atmire NV
 

 

Răsfoiește

În tot DSpaceComunități; ColecțiiDupă data publicăriiAutoriTitluriSubiecteAceastă colecțieDupă data publicăriiAutoriTitluriSubiecte

Contul meu

Conectare

DSpace 6.0 | Copyright © Arthra Institutional Repository
Contactați-ne | Trimite feedback
Theme by 
Atmire NV